Draco Electric Metal sheer knife
Item number
CSU08780200
Local code:
*
GTIN:
3606481112668
Description:
Draco Electric Metal sheer knife
Wibe Group. CSU08780200 - Stago - Draco Electric Metal sheer knife
Properties
Status product
Product status
Commercialized
Commercial and Web
Short description
Draco Electric Metal sheer knife
Medium description
Stago - Draco Electric Metal sheer knife
Material
Steel
Material type or surface treatment
Painted
Environmental corrosion class
C2
Base
Activity
Cable support systems
Product family
Cable trays
Brand
Stago
GTIN
3606481112668
ETIM (EC000017-Explosion proof CEE-plug/-coupler)
Mains voltage (EF000105)
* V
Nominal current (EF000001)
* A
Number of poles (EF001391)
*
Voltage according to EN 60309 (EF006726)
*
Clock hour position (EF006584)
* h
Identification colour (EF006725)
*
Model (EF000010)
*
Material housing (EF001596)
*
Cable entry (EF000537)
*
Protective contact (EF001033)
*
Contact material (EF004019)
*
Surface treatment contacts (EF002558)
*
For Ex (EF005728)
*
For Ex (EF008404)
*
Ex (EF000854)
*
Logistic
Quantity pack 1
1
Weight pack 1
.068 kg
Length pack 1
200 mm
Width pack 1
120 mm
Height pack 1
12 mm
Customs code
82130000
Net weight
.07 kg
Country of origin
NL
Certification
ETIM class
EC000017
Product downloads
Environmental Documents
Downloads
Environmental Products
Corrosion class | C1 | C2 | C3 | C4 | C5 | CX | |
Environmental corrosion | Very low | Low | Average | High | Very high | Extreme | |
Examples of environments | Indoors | Heated areas with arid atmosphere and insignificant quantities of pollutant, e.g. offices, shops, schools and hotels. | Non-heated areas with fluctuating levels of temperature and humidity. Few instances of condensation and low levels of airborne pollution, e.g. sports halls and warehouses. | Average levels of humidity and some airborne pollution resulting from production processes, e.g. breweries, dairies, laundries. | High humidity and considerable airborne pollution as the result of production processes, e.g. chemical plants, swimming pools and dockyards. | Buildings with almost permanent condensation and with high pollution | Industrial buildings with extreme humidity and aggressive atmosphere. |
Outdoors | Atmospheres with low levels of airborne pollution. Rural areas. | Atmospheres containing some salt or average levels of air-borne pollution. Urban and light industrial areas. Areas affected by coastal conditions. | Atmospheres with average salt content or discernible levels of airborne pollution. Industrial and coastal areas. | Industrial areas with high humidity and aggressive atmosphere, and coastal areas with high salinity | Offshore areas with high salinity, industrial areas with extreme humidity, and aggressive atmospheres, sub-tropical or tropical atmospheres. | ||
Wibe Group designation
Recommended Very high durability (>20 years)
Possible alternative. High durability (10-20 years)
|
Electro-galvanized (EG) |
|
|
||||
Pre-galvanized (PG) |
|
|
|
||||
Zinc+ (Z+) |
|
|
|
|
|||
Hot-dip galvanized (HDG) |
|
|
|
|
|
||
Zinkpox (ZP) |
|
|
|
|
|
|
|
Stainless steel AISI 304L(SS304) |
|
|
|
|
|
|
|
Stainless steel AISI 316L (SS316) |
|
|
|
|
|
|
|
Glass Fibre Reinforced Polymer (FRP/GRP) |
|
|
|
|
|
|
This table shows estimated values.
For more detailed advice, please contact technical support at Wibe Group