Flat Elbow 45° LM100 150 R9 PC1
Item number
MLF1439R9PC1
Local code:
*
GTIN:
7321678044091
Description:
Flat Elbow 45° LM100 150 R9 PC1
Properties
Commercial and Web
Short description
Flat Elbow 45° LM100 150 R9 PC1
Medium description
Flat Elbow 45° LM100 150 R9 PC1
Length
877 mm
Width
482 mm
Height
100 mm
Base
Activity
Cable support systems
Product family
Cable ladders
Brand
Mita
Range
Flex
GTIN
7321678044091
ETIM (EC001535-Bend for cable ladder)
Change of direction (EF005210)
*
Type of side joist (EF007666)
*
Side wall perforation (EF001122)
*
Type of rung (EF001060)
*
Angle (EF001218)
*
Bend model (EF020423)
*
Hinging (EF001076)
*
Cable ladder height (EF004818)
* mm
Cable ladder width (EF004817)
* mm
Model (EF000010)
*
Inner radius (EF004793)
* mm
Wide span model (EF006397)
*
Suitable for circuit integrity (EF007806)
*
Material (EF002169)
*
Material quality (EF001257)
*
Surface protection (EF000139)
*
Colour (EF000007)
*
RAL (EF000116)
*
Logistic
Customs code
39169010
Net weight
3.8 kg
Country of origin
Malaysia
| Corrosion class | C1 | C2 | C3 | C4 | C5 | CX | |
| Environmental corrosion | Very low | Low | Average | High | Very high | Extreme | |
| Examples of environments | Indoors | Heated areas with arid atmosphere and insignificant quantities of pollutant, e.g. offices, shops, schools and hotels. | Non-heated areas with fluctuating levels of temperature and humidity. Few instances of condensation and low levels of airborne pollution, e.g. sports halls and warehouses. | Average levels of humidity and some airborne pollution resulting from production processes, e.g. breweries, dairies, laundries. | High humidity and considerable airborne pollution as the result of production processes, e.g. chemical plants, swimming pools and dockyards. | Buildings with almost permanent condensation and with high pollution | Industrial buildings with extreme humidity and aggressive atmosphere. |
| Outdoors | Atmospheres with low levels of airborne pollution. Rural areas. | Atmospheres containing some salt or average levels of air-borne pollution. Urban and light industrial areas. Areas affected by coastal conditions. | Atmospheres with average salt content or discernible levels of airborne pollution. Industrial and coastal areas. | Industrial areas with high humidity and aggressive atmosphere, and coastal areas with high salinity | Offshore areas with high salinity, industrial areas with extreme humidity, and aggressive atmospheres, sub-tropical or tropical atmospheres. | ||
|
Wibe Group designation
Exceeds requirements. Extremely high durability.
Recommended very high durability ( >20 years)
Possible alternative. High durability (10-20 years) |
Electro-galvanized (EG) |
|
|
||||
| Pre-galvanized (PG) |
|
|
|
||||
| Zinc+ (Z+) |
|
|
|
|
|||
| Hot-dip galvanized (HDG) |
|
|
|
|
|
||
| Zinkpox (ZP) |
|
|
|
|
|
|
|
| Stainless steel AISI 304L(SS304) |
|
|
|
|
|
|
|
| Stainless steel AISI 316L (SS316) |
|
|
|
|
|
|
|
| Glass Fibre Reinforced Polymer (FRP/GRP) |
|
|
|
|
|
|
|
This table shows estimated values.
For more detailed advice, please contact technical support at Wibe Group